RUBBER TEST CENTER |
Provides various types of mixed rubber with different properties, such as natural rubber, ethylene propylene rubber, nitrile rubber, chloroprene rubber, hydrogenated nitrile rubber, fluorine rubber, acrylate rubber, etc., to meet the needs in Various automotive parts |
testing items
|
properties
|
Testing standards |
Hardness, Shore A/degree
|
50~80
|
GB/T531-1999 |
Minimum tensile strength/MPa
|
18~22
|
GB/T528-1998 |
Minimum elongation at break/% |
≥350
|
GB/T528-1998 |
tear strengthKN/M
|
10~40
|
GB/T529-1998 |
Maximum compression permanent deformation/%,B型100 ℃×22h
|
≤50%
|
GB/T7759-1987 |
Hot air aging 100 ℃×70h
|
|
|
Hardness, Shore A/degree
Minimum tensile strength
Minimum elongation at break%
|
0~±15
±-30
-50
|
GB/T531-1999
GB/T528-1998
GB/T528-1998 |
brittleness temperature℃
|
≤-40
|
GB1682 |
ozone resistance
|
200pphm,72h,40℃,20%:0级
|
GB/T7762-2003 |
Fatigue performance
|
with a radial force of 15KN and a frequency of 2HZ. There are no cracks on the rubber after 600000 cycles
|
|
|